This company has announced the availability of Multicore HF108, a lead-free, halogen-free solder paste that combines all of the benefits of robust lead-free materials with the advantage of no deliberately added halogen.

Though industry consortia have set some competing standards as to the acceptable levels of halogen, the common benchmark is up to 900 ppm bromine, 900 ppm chlorine and maximum total halogens of 1500 ppm.   Henkel, however, has developed a material that has zero deliberately added halogens, yet has the excellent reflow and stability characteristics normally associated with halogen-containing materials.

Multicore HF108 also has excellent high-speed print capability, a long and stable shelf-life of up to six months when refrigerated or four weeks at room temperature, and a wide process window. Performance is robust and comparable to other Henkel market-leading lead-free formulations, but without any added halogens.

For more information, visit www.henkel.com/electronics.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40