The guide provides bond strength data for substrates such as ABS, delrin, nylon, polycarbonate, polypropylene, polyethylene and PVC. In addition, it presents shear strength data on 23 Loctite adhesives, including cyanoacrylates, epoxies, hot melts, light-cure acrylics, polyurethanes, silicones and no-mix/static-mix acrylics.
For more information, phone (800) LOCTITE or visit www.henkelna.com/loctitestructurals.