Three high-performance REACH-compliant epoxy adhesives are now available for use by aerospace manufacturers and component suppliers for fabrication, assembly, and repair. The products reportedly comply with federal regulations and are qualified to OEM specifications governing the performance properties of materials used to build and maintain commercial and corporate/private aircraft, as well as helicopters.

Araldite® EP 1000 A/B epoxy adhesive is a nano-toughened structural adhesive paste that reportedly features very high lap shear strength and good peel strength at temperatures of up to 250ºF (121ºC). The translucent epoxy can withstand exposure to aviation fuels and hydraulic fluids.

Araldite AW 4859/Hardener HW 4859 epoxy adhesive is formulated for bonding composite aircraft structures such as stringers, ribs, spars and flight control surfaces. The epoxy reportedly produces joints with excellent hot/wet strength, a service temperature of up to 284ºF (140ºC), and good moisture and chemical resistance. Supplied in convenient dual-barrel cartridges and bulk containers, the toughened black adhesive is sag resistant and gap filling.

Araldite 1570 FST A/B epoxy adhesive is a flame retardant, halogen-free, black paste for use in bonding and repairing cargo panels, as well as other composite and thermoplastic components used in aircraft interiors. The system meets flame, smoke and toxicity standards, including FAR 25.853 (a) and (a-1) and AITM 3.0005, and is qualified to an Airbus specification. Lap shear strength of the room temperature cure material is more than 2,400 psi.

For more information, phone (281) 719-4859 or visit www.huntsman.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40