The CFS 5 HD-S High Dispersion Air Classifier with a gas flow volume of 50 m3/h (approximately 29 SCFM) guarantees optimal classifying results on a laboratory scale. Low volume and/or high value materials can be classified on this new laboratory-size mill. The easy-access and, consequently, easy cleaning of the machine is ensured by an accessible design with all parts completely removable. A complete classifier system can be provided with a feeder, cyclone, filter, blower and control panel installed on a base frame at an attractive price. As a further option, a CGS 10 Fluidized Bed Jet Mill can be installed on the base frame to provide a complete and totally flexible laboratory system.

For more information, visit http://www.netzschusa.com .

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI July 2014 cover

2014 July

Our annual Distributor Directory helps you locate a distributor that best suits your needs. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px