“Escalating and volatile pricing for titanium dioxide has been an important issue for PPG,” Kahle said. “PPG possesses intellectual property and expertise in the production and finishing of titanium dioxide pigment, and we intend to leverage this and engage with potential partners to develop innovative supply solutions.”
According to Kahle, PPG previously manufactured chloride titanium dioxide at its Natrium, WV, chemicals plant. He said that PPG anticipates the initiative may include technical collaborations, joint ventures, licensing, technical assistance opportunities or other strategic commercial initiatives.