nusilMED-6219 is an optically clear, high-durometer elastomer designed to cure at a range of temperatures. With low viscosity, it is a naturally flowable and self-leveling material.

Due to its transparent appearance, MED-6219 can be used for potting and encapsulating electronic devices or for making molded parts. Because it can be vulcanized at both high and low temperatures, this elastomer is reportedly suitable for temperature-sensitive substrates or for use in environments with fluctuating temperatures.