Kerabond T is a new non-sag, non-slump mortar that can be used in thin-set and medium-bed tile installations on interior/exterior residential and commercial floors and walls.MAPEI mortar When mixed with water, the mortar reportedly acts as a medium-bed mortar meeting the ANSI A118.1 standard and ISO 13007 Classification C1T.

When mixed with Keralastic™, a second-generation “flexible” acrylic latex additive from MAPEI, the resulting system reportedly has exceptional bond strength, flexural strength, elongation characteristics and freeze/thaw durability, meeting the ANSI A118.15 standard and ISO 13007 Classification C2ES2P2.