A new water-based reactive auto-deposition coating is now available from this company. Bonderite® M-PP 930C™ was reportedly formulated specifically to deliver a uniform, defect-free surface coating on raw cast components and ferrous metals. The epoxy-acrylic urethane coating can easily coat both the inside and outside of complex components, and delivers enhanced corrosion and abrasion resistance, excellent thermal stability, and superior edge protection, abrasion resistance, and flexibility.

Depending on the type of substrate and cleanliness of the metal, application of the coating can be as simple as a seven-step, room temperature deposition process that requires no electrical contacts and involves a chemical reaction between the water-based organic emulsion and the metallic surface. The low-energy process uniformly coats large volumes of fully assembled, densely racked or complex-shaped metal parts.