Ellsworth Adhesives Europe now offers 3M’s expanded line of VHB Tape RPXX. The new products will reportedly include five different calipers with both paper and filmic liner variants.

The filmic liner is available on RP16F, RP25F, RP32F, RP45F and RP62F in log roll format only. Filmic liners are reportedly preferable for some converting processes such as level winding or intricate die cuts.