Despite a challenging
economy and declining production, the polyurethane industry continued to evolve
over the past two years while addressing growing concerns over energy
conservation, according to the 2008 End-Use Market Survey on the Polyurethanes
Industry in the United States,
Canada and Mexico.
Research conducted by IAL Consultants on
behalf of the Center for the Polyurethanes
Industry (CPI) of the American Chemistry Council, shows that overall
production of polyurethane in NAFTA declined by 6.7% per year during the past
two years. The figure reflects a 7.7% annual decline in U.S. markets and 10.8% decline in Canada, while Mexico has shown positive growth
for the third consecutive survey. The production of polyurethane in Mexico
increased at an average annual rate of 9.6% over the past two years, partly due
to increased domestic demand.
“With the dip in automotive output, decreased consumer
spending, high levels of imported furniture and a drop-off of activity in new
housing starts, we were prepared to see a decline in polyurethane production in
the U.S. and Canada,” said Neeva-Gayle Candelori, Director of CPI.
“Overall, our research shows that the industry continues to
change,” said IAL Associate Director Angela Austin. “While some markets
are mature, new ones have opened up. Renewable chemicals and energy
efficiency continue to be important topics. Change is essential for
evolution and it would be worrying if there were no signs of market evolution.”
Changing Markets
Signs of growth in the
polyurethane industry included continued increases in spray polyurethane foam
demand for residential and industrial applications, as well as use of the
material by the U.S. Army to insulate tents and other structures at bases in the
Middle East. Polyurethane also is being
used for effective wound dressings, pharmaceutical delivery media, reliable
drug delivery, comfortable mobility aids, and hygienic hospital
environments. The demand for low VOC and high performance coatings related
to product substitutions made the decline in the production of coatings,
adhesives, sealants and TPU less severe.
Though there was a sharp
decrease in binder production as a result of the decline in OSB (oriented
strand board) demand by the U.S.
housing sector, the desire for safe and clean recreational areas has helped
increase use of polyurethane binders in sports tracks and playgrounds in the
past two years. New applications to improve quality of life are
contributing to market evolution as well, such as new comfort levels in golf
cart seating for the growing number of elderly.
Manufacturers looking to
comply with new regulations and secure certification are also finding ways to
create opportunities for growth. The survey shows a boost to the rigid polyurethane
foam market for thicker panels needed to meet new ASHRAE (American Society of Heating,
Refrigerating and Air-Conditioning Engineers) standards. CARB
(California Air Resources Board) regulation and
the CertiPUR program also helped to secure
business in the bedding industry for flexible polyurethane foam.
Differences by Region
The U.S., representing 81% of the total
polyurethane production in NAFTA, had a market breakdown similar to NAFTA
overall. Imports of upholstered furniture continued to increase in the U.S.
Though statistics from the U.S. Department of Trade and Commerce did indicate a
slight drop in overall imports during the past two years, these were a
reflection of the current state of the housing market and declining consumer
demand.
In Mexico, production of rigid
polyurethane foam dominated the market as new companies invested in the country
and the appliance industry continued to grow. In 2008, the Mexican
appliance industry produced 9 million refrigerators and freezers compared to
11.3 million in the U.S.
Mexican furniture and
automotive markets also grew during 2008, driven by export and domestic
demand. With 2.1 million units in 2008, automotive production exceeded Canada’s.
Flexible molded foam end-use production increased due to the manufacture of
automotive components and flexible slabstock production increased, as
well. Though families currently prefer to buy new upholstered furniture
over new mattresses, the bedding market has potential for further
development. Despite a deficit of 5 million homes in Mexico, home
ownership has increased.
Canada’s
dependence on the U.S.
resulted in a greater production decline than experienced in the U.S.
The country was the third market in the NAFTA region and accounted for 8.9% of
total production. Flexible foam slabstock accounted for 16% of total
production, compared to 21% in 2006 and the fall in U.S. housing starts led to 54% of
OSB production being idled.
As an environmentally
conscious country, the population continued to buy products marketed as
“eco-friendly”, such as rigid polyurethane foam and flexible polyurethane foam.
Rigid polyurethane foam accounted for 39% of production in 2008 compared
to 28% in 2006, another sign of interest in greater energy efficiency.
In the energy sector,
components made from polyurethane cast elastomers, technical insulation
coatings and sealants received increased capital expenditure for maintenance
and development, mainly as a response to the high oil prices of 2007 and the
first half of 2008.
Select Market and Product Highlights
Product types:
Once again, rigid polyurethane foam products accounted for the largest share of
the 6.5 billion pounds of polyurethane produced in NAFTA in 2008. The
figure reflects the relative strength in demand for rigid polyurethane foam as
an insulation material. The past two years have witnessed stable demand
from the construction industry.
Construction:
New housing starts have declined, but expenditures on remodeling and repairs
increased. This development is largely responsible for the growing demand
for spray polyurethane foam as internal wall insulation and the slower than
expected decline in CASE products like elastomers used in thermal breaks in
insulated windows, solar panels, wooden floor and turbine blade coatings,
adhesives and sealants, and the steady demand for one component spray
foams. The versatility of spray polyurethane foam also has contributed to
its use in army tents and structures in the Middle East
where it has contributed to fuel savings.
As part of its industry-wide
survey, IAL looked in depth at the factors affecting the declining demand for
flexible polyurethane foam in the automotive, furniture and bedding industries:
Furniture/Bedding:
U.S.
production of flexible slabstock foam fell sharply from 2006 - 2008.
Flexible foam stock production dropped by nearly 25% in 2008 compared to
2007. The main impetus behind this decline is the decrease in furniture
production due to lack of consumer demand and imports. Imports of
upholstered furniture continued to rise until the end of 2007. The rate
of imports is not expected to change in the near future as U.S. government
incentives to first-time homebuyers will likely go towards imported goods.
The bedding sector continued
to use large volumes of flexible polyurethane foam during 2008. Mattresses
manufactured in the U.S.
used more foam per unit for deeper mattresses with softer toppers; more hybrid
mattresses were produced, as well. Since the end of 2008, factors such as
the reduced cost of lower density foams, thinner mattresses, and customers
requiring faster delivery times for mattresses than other furniture delivery (2
-5 days), have helped protect the industry from imports.
Transportation:
While the automotive industry has experienced significant downsizing, it has
also seen an increased demand for more economical vehicles. Production
fell by 3.1 million since 2006, but there are now roughly 8 million flexible
fuel vehicles on U.S.
roads and more are expected in the future. Polyurethane foam used in
automotive seating has trended toward becoming thinner, while density is
increasing, offering more cabin space above the seat and allowing the required
amortization of vibration. The decline in molded seat foam is related to
the general downtown in automotive production.
“It’s both a challenging and
exciting time for the polyurethanes industry,” says Candelori. “By
responding to consumer needs and legislation, and improving safety, there are
many opportunities for the industry to find new ways to improve people’s
quality of life.”
Says Austin, “We remain
hopeful that while total production volumes have been low, research and
development continue and that the polyurethanes industry will have a raft of
new products and applications by the next survey.”
Conducted every two years,
the CPI End-Use Market Survey addresses the North American polyurethanes
industry. Angela Austin of IAL Consultants presented the major findings
of the survey to a group of influential scientists, engineers, manufacturers
and business leaders from around the world at the closing session of the
Polyurethanes 2009 Technical Conference in National Harbor, Maryland.
IAL Consultants interviewed
more than 200 organizations and companies in North America,
including end-users, formulators and producers, to complete the survey.
The End-Use Market Survey is available for purchase at
www.americanchemistry.com/polyurethane. New for this year, CPI is
also offering an interactive downloadable database where users can access
survey data. For further information or to purchase the survey, contact
Neeva-Gayle Candelori, CPI at (703) 741-5103.