To meet international market demand, this company has developed new, optically clear pressure sensitive technologies for the display-screen industry. Arclear™ pressure sensitive adhesives offer high-performance, defect-free technology that does not require curing. The products are available in either transfer-adhesive or custom-coated film format. The technology delivers an isotropic, non-birefringent adhesive of minimal thickness (25 m) with transmission values greater than 95% and superior humidity-, heat-, cold- and shock-resistant parameters.