Adhesives Research: PSA Products
September 11, 2000
This company has introduced its new line of ARclean™ acrylic acid and organotin-free, strippable, electronically clean, pressure sensitive adhesive products. These products minimize contamination and corrosion in electronic applications such as higher-end hard disk drives. These PSAs do not contain acrylic acid, a common building block of many industrial PSAs, which can cause head corrosion and media fogging.