ADMTronics Unlimited offers a unique, water-based additive, Polaqua AD, that improves the performance of any aqueous adhesive, paint, coating or resin.

ADMTronics Unlimited, Inc., Northvale, N.J., offers a unique, water-based additive, Polaqua AD, that improves the performance of any aqueous adhesive, paint, coating or resin. Even minor product additions improve flow and lay down. Its high lubricity allows enhanced pumping of any liquid, from water to pigment slurries. Additions are from 1% to 10% by weight, depending upon the type of liquid and degree of change desired.