MACTAC

This company's PermaFlex(r) family of rigid over-laminating films, including PermaFlex IP6000, IP6100 and IP6200, now features a new, very aggressive adhesive designed to eliminate tunneling on exhibit images. PermaFlex products also lend rigidity to photos, transparencies and printed images for use in flat or curved display configurations. After lamination with PermaFlex, the image may be rolled and transported on a regular basis. This is due to PermaFlex's high-shear adhesion ability, even under stress. Circle No. 115