A new formulation of Ashland’s ENVIREZ
® resin technology can now be used for pultrusion applications. ENVIREZ 50380 resin features high reactivity that supports fast line speeds.
ENVIREZ 50380 resin contains recycled materials and contributes to LEED points under Materials and Resource Credits 4.1 and 4.2. Ashland first introduced ENVIREZ resin in 2002 for use in sheet molding compound, and has since expanded the range of product applications to include hand lay up, infusion molding, and solid surface products.