SUPASILTM is a new range of fumed silica powders to be used primarily to thicken products that have low viscosity. In addition, the powders can also be used as anti-caking and anti-sagging agents.

SUPASIL powders are white, non-toxic particles of micronized silica. Their size is tightly controlled and can be produced in grades from 7 to 40 nanometers wide, which in turn have specific surface areas of 70-400 m²/g.