German researchers have taken inspiration from nature to create a dry adhesive material that sticks to the smoothest of surfaces.
People have long marveled at
the ability of creatures such as insects and certain lizards to climb up
vertical walls and even walk across ceilings without falling off. Recently,
research has shown that these animals owe their ‘stickiness’ to the presence of
extremely fine hairs on their feet, which optimize contact with surfaces. Many
people have tried to reproduce these systems, but until now the resulting
artificial materials have had a limited lifecycle and were simply not as sticky
as the natural versions.
Now, researchers from the Max Planck Institute for Metals Research and Gottlieb
Binder, a company specializing in attachment systems, have successfully
produced an adhesive material whose microstructure is based on the soles of
insects’ feet. Their findings are reported in the early online edition of
Journal
of the Royal Society Interface.
In this case, the insects in question were beetles of the family Chrysomelidae,
which are known to be experts in the art of sticking to very smooth surfaces.
The ‘hairs’ of the new material resemble tiny mushrooms; a thin plate 40
micrometres in diameter sits atop a pillar which has a sturdy base but a narrow
neck and is 100 micrometers high. The ‘mushrooms’ are arranged hexagonally on the
surface of the material.
The material was made by pouring a polymer mixture into a mold and waiting for
it to set before carefully removing the material from the mold. According to
the researchers, the creation of the mold, with its delicate microstructure,
was incredibly challenging, and the details of the process are a closely
guarded secret. Creating the polymer mixture was also difficult; mixtures that
were too liquid simply flowed out of the mold, while mixtures which were too
viscous were unable to penetrate into the fine microstructure.
A battery of tests revealed that five square centimeters of the material are
able to stick objects weighing up to 100 grams to a smooth wall. The material
can be used several times without losing stickiness, and if it gets dirty,
simply washing it in soapy water will restore its adhesive qualities.
Furthermore, it does not leave behind visible marks when removed from a
surface.
The material does not perform as well on rougher surfaces, which does not
surprise the researchers. “Insects also have difficulties walking on surfaces
that are slightly rough,” explained project leader Stanislav Gorb of the Max
Planck Society. “This is a fundamental problem of the adherence mechanism.”
The researchers credit the success of their system down to a number of factors.
The thin plate at the top of the ‘mushroom’ is flexible enough to form a
reliable contact with the surface, even in the presence of small particles of
dirt. Meanwhile, larger particles are able to slip into the space between the
pillars where they do not affect the ability of the plates to stick to the
surface. The thin neck of the pillar also offers flexibility in the face of
uneven surfaces. Finally, broken pillars do not alter the effectiveness of
neighboring pillars.
The scientists describe their work as “a considerable step towards the
development of an industrial dry adhesive.” The new material could be used in a
protective tape for sensitive glass surfaces, or in reusable pads for the
attachment of small objects to smooth surfaces. It has already been attached to
the feet of a robot, which was subsequently able to walk up a vertical glass
wall. The researchers now plan to improve the ‘stickiness’ of their material by
refining its structure.
For more information, visit www.mpg.de/portal/index.html or
www. www.journals.royalsoc.ac.uk/.
Source: CORDIS NewsLinks