BROOKFIELD ENGINEERING: Rheometer
May 22, 2001
This company introduces the R/S rheometer for rheological evaluation of materials through the direct measurement of viscosity, yield stress and thixotropic response.
This company introduces the R/S rheometer for rheological evaluation of materials through the direct measurement of viscosity, yield stress and thixotropic response. Designed to provide controlled stress and shear-rate analysis, the unit is available with cone/plate, plate/plate or coaxial cylinder measurement geometry. Powerful flow-characterization tools include shear ramp, loop and single-point testing.