Adhesives Magazine

BROOKFIELD: Texture Software

September 29, 2008

This company’s new TexturePro CT Software is specifically designed for use with the new CT3 Analyzer, which connects directly to any USB port on a user’s computer.

The program allows users to collect data and perform detailed analysis on test samples of various shapes and sizes with real-time graphic plotting during the test. Custom reports and graphs are easily created from the menu screen, and the sample identification set-up screen helps new operators get started with test fields that outline a variety of parameters.

The software features advanced data analysis with built-in parameter calculations such as springiness, chewiness, hardness and much more, helping new users select the best data analysis for their specific test.

New TexturePro CT also has an optional Secure Mode that enables the operator to run new test methods, collecting and saving data while protecting existing test methods and data against change or deletion.

For more information, visit www.brookfieldengineering.com.