Adhesives Magazine

Cleaning Solvent

September 24, 2001
DYNALOY INC.
Dynasolve SF-30 fluid is a volatile silicone fluid that has a range of uses in specialty cleaning and carrier applications. It is suitable for removal of silicone oils and uncured silicone materials, and for use as a base fluid or carrier solvent. It provides excellent detackification, spreading and leveling properties. The product also exhibits low toxicity, low odor, quick evaporation rate, low surface tension and no VOCs. Circle No. 101