Adhesives Magazine

Conductive Epoxy Adhesive

February 27, 2002
CREATIVE MATERIALS INC.

This company's 122-07 is a screen-printable, B-stageable, thermally conductive epoxy adhesive. The product remains electrically insulating while exhibiting a high degree of thermal conductivity. The system features excellent thermal stability, outstanding chemical resistance and excellent high-temperature properties. Circle No. 121