Controlling a Sticky Situation (11/24/10)
November 24, 2010
It may be possible to control the level of an adhesive's stickiness from an external stimulus. A polymer film stuck to a hydrogel surface swells when it absorbs water, thus increasing its adhesion properties.
Click here to read the full story.