MCI®-2018 V/O is a higher viscosity version of the company’s MCI®-2018 sealer for vertical and overhead applications. This 100%-active silane line of water repellants works by chemically reacting with concrete surfaces to form a strong bond with the substrate. The product creates a hydrophobic layer that repels water and keeps chlorides out without affecting the moisture vapor transmission of the concrete.
The sealer can be applied via spray, brush or roller. The increased viscosity of the sealer reportedly makes it easy to apply to bridge supports, garage pillars, or building walls without wasting product through spillage.