Cotronics: Flexible, Conductive Epoxy
July 25, 2000
New Duralco™ 125N stress-free epoxy forms flexible, electrically conductive bonds for continuous use up to 400ºF. The product cures at room temperature to form bonds with excellent resistance to most chemicals, solvents and moisture. Applications include flexible circuits, solder replacement, bonding semi-conductors, EMI shielding, wire tracing and heating-element assembly.