A new line of anisotropic conductive adhesives is now available. Offered in paste form, as films, and in a recently introduced line of anisotropically conductive pressure-sensitive tapes, the adhesives can be used in RFID manufacture, for flat-panel displays, and in the assembly of semiconductor modules. The applications are myriad, and new lower temperature and faster curing methods have reportedly increased the breadth of applications. The adhesives reportedly can provide superior conductivity, excellent adhesion to a variety of substrates, and are less sensitive to handling and extremes in ambient conditions.