125-26A/B119-44 is an electrically conductive fine-line flexible two-part epoxy ink for the printed electronics industry. Available as a two-component system, the ink reportedly features excellent adhesion to substrates including transparent conductive oxides and low-surface-energy substrates. In addition, it is resistant to scratching and creasing.