Devcon 10 Minute Epoxy is a self-leveling adhesive formulated for bonding, potting, and cosmetic repairs in a variety of OEM applications. Available in clear and black formulations, the epoxy has a 10-minute working time and a fixture time of 20 minutes. Functional cure is attained in 90 minutes. Once cured, it provides a tensile shear strength of 2,400 psi (as measured on grit-blasted steel with a bond-line thickness of 0.010 inch, per ASTM D1002) and a peel strength of 20-25 pli. Bonds withstand service temperatures from -67 to 200 degrees F (dry). Both formulations are 100% solids with very low VOC emissions, and both are mixed as dispensed using hand-held manual or pneumatic dispensers with static mixing nozzles. The mixed viscosity of the clear formulation (80,000 cps) is higher than that of the black formulation (70,000 cps).