DOW CORNING: Silicone Release Coatings

December 19, 2004
Dow Corning Corp. has introduced a low-cost, solventless, silicone release coating line designed to help customers defend themselves against rising platinum prices and other cost-related issues without sacrificing performance. Syl-Off Advantage Series release coatings enable significantly lower platinum usage - 20-50 ppm vs. the 100 ppm or more that conventional systems require. Syl-Off is a complete solventless, platinum-catalyzed, thermal-cure release coating system. It includes a comprehensive selection of base polymers, crosslinkers, release modifiers and catalysts that enable flexible control of cure characteristics, release profile, and costs. Two versions of the system are available to accommodate different needs.