9440-A/B cures to depth in seconds upon exposure to UV/visible light
to provide protection to electronic components and circuitry. It is a
UV/visible light-curable silicone potting and sealing material designed for
applications where fast cure, enhanced thermal performance, and
room-temperature shadowed-area cure are required. Cure-Point 9440-A/B has a >90 day room temperature mix life.
This product is designed to withstand
long exposure to temperatures ranging from below -40°C to above 200°C while
retaining fast-cure processing benefits associated with UV-curable materials. This
makes it superior to RTV silicones and heat-cure silicones which require longer
cure times or elevated temperatures to cure. Cure-Point 9440-A/B excels in applications where oil or chemical
exposure are present. It also features a fast, tack-free cure with negligible
shrinkage.
DYMAX UV/visible
light-curable materials are solvent free and their ability to cure in seconds
results in lower processing costs. When cured with DYMAX light-curing spot lamps,
focused beam lamps or flood lamps, they deliver optimum speed and performance
for maximum efficiency. This product is in full compliance with the RoHS
Directives 2002/95/EC and 2003/11EC.