DYNALOY: Cleaning Solvent
April 1, 2001
Poly-Flush can be used for flushing polyurethane, polyester, epoxy, acrylic and other two-component materials. It was developed as a more effective replacement for DBE, citrus-based and other low-cost flushing solvents. It is a low-toxicity, non-chlorinated, non-flammable solvent capable of replacing hazardous and/or flammable solvents.