Eastman Chemical Co. now offers its Eastoflex APOs (amorphous polyolefins) in convenient, easy-to-handle pellets. Eastoflex APOs are widely used as base polymers in the formulation of hot-melt adhesives, sealants, paper laminations and pressure-sensitive adhesives. They are also suitable for rubber compounding and waterproofing compounds for wire and cable applications, as well as for use as a modifier for asphalt in single-ply roofing.