June 2, 2003
Elastomers
TRANSENE CO.
This company has introduced Translastic RTV Silicones, elastomers designed to stabilize and insulate electronic components and circuit modules. Available in a range of viscosities, the silicones impart protection against temperature extremes, moisture, contamination, weathering, corona, corrosive environments, mechanical shock and vibration. Operating temperatures as high as 250 degrees C are achievable.