A new epoxy potting compound meets NASA’s outgassing requirements. The material, 20-3652, is a filled epoxy casting, potting and encapsulating resin system. It is a dielectric-grade epoxy that reportedly exhibits excellent physical, thermal and electrical insulation properties.
For more information, visit
www.epoxies.com.