Epoxy Monomer<br>INDSPEC CHEMICAL CORP.
April 17, 2003
Epoxy Monomer
INDSPEC CHEMICAL CORP.
This company has developed diglycidyl ether of ethoxylated resorcinol (DGER), a resorcinol-based epoxy monomer for use in high-performance applications. DGER offers a balance of good flexibility, low viscosity and high curability with various epoxy-curing agents.