Filter Media
BBA FILTRATION
Reemay X-Treme is a pleatable, multi-denier polyester spunbond media that offers dust-holding capacity and low pressure drop. This product is a nonwoven web that consists of multiple layers of polyester fibers that can be varied in composition to meet specific application requirements. Denier per filament can also be varied between the layers to provide exacting filtration properties.