MOX®-Tape products are a family of self-fusing silicone rubber tapes that deliver superior electrical insulation in harsh service environments. The products are used to form cohesive barriers that resist moisture, oxygen, ozone and corona over a temperature range of -65ºF to 500ºF. These tapes deliver a minimum dielectric strength of 300 volts/mil at 356ºF, and a volume resistivity of at least 1013 ohm/cm, making them well suited to aerospace, automotive, heavy truck and electrical applications.