Garlock Sealing Technologies now offers a six-page brochure on its new Sage GYLON
® gaskets for severe chemical services. Supplied in discrete-cut form, this high-performance PTFE gasket provides superior load retention, permeability, sealability and resistance to a broad range of hazardous chemicals. Covered in the brochure are physical properties including temperature, pressure, sealability, creep relaxation, recovery, tensile strength, modulus of elasticity, specific gravity, dielectric strength and gas permeability. Also provided are compatibility with more than 500 different chemicals and test data including hot compression, HOBT2 test results and bolt torque values.