The ARclad 3600 Series is a line of gray-colored, expanded cellular foam glazing tapes. The glazing tapes are coated on both sides with a high-strength, acrylic-based pressure sensitive adhesive. The adhesives are ideally suited for sealing window assemblies in substrates such as plastics, vinyl, metals and construction materials, including glass and preserved wood.