Greening The Process (2/11/11)

February 11, 2011

Studies have shown that a newly discovered catalyst can convert lactic acid into acrylic acid in a more efficient and environmentally friendly way. Acrylic acid is a key material that is traditionally used in paints, adhesives, textiles and many other products.

Click here to read the full story.