Adhesives Magazine

GRIEVE CORP.: Walk-In Oven

May 13, 2008

No. 950 is a 350°F gas-heated walk-in oven currently used for bonding composite materials inside molds. Workspace dimensions of this oven measure 10’W x 20’D x 8’H.  700,000 BTU/HR installed in a modulating natural gas burner provides heat while a 24,500 CFM, 20-HP recirculating blower provides a combination airflow to the workload.

The Grieve walk-in oven features 4” insulated walls, aluminized steel interior and exterior, heavy-duty double doors, and a 1/4” steel plate floor.

All safety devices required by IRI, FM and NFPA Standard 86 for gas-heated equipment can be found on No. 950, including a 6500 CFM powered forced exhauster.  Also included is a recording and programming temperature controller, plus motorized dampers on the air intake and exhaust for accelerated cooling.

For more information, visit www.grievecorp.com.