H.B. Fuller Co. recently announced it has received notification from NSF International for its UR3501 A/B two-part adhesive for spiral wound membrane bonding for reverse osmosis (RO) filtration. The product has been tested and certified by NSF to NSF/ANSI Standard 61 - Drinking Water System Components - Health Effects. This certification adds to H.B. Fuller’s NSF certification of two of its potting compounds (FE7811 Epoxy and UR2187 Polyurethane) for hollow fiber water filtration.
“This NSF International certification represents our continuing and deepening commitment to the membrane separation industry,” said Matt McGreevy, business director. “We strive to provide our customers with every advantage in meeting industry requirements.”