Henkel
Corp. has introduced Loctite® 263™ threadlocker, a high-strength,
single-component anaerobic threadlocker designed to permanently lock and seal
threaded fasteners up to one-inch in diameter. The high-viscosity, primerless,
red threadlocker cures on fasteners treated with thread lubricants and
anti-corrosion/protection fluids without cleaning.
When
confined in the absence of air between close-fitting metal surfaces, it
fixtures and cures rapidly. The anaerobic threadlocker performs equally on both
active and passive metal surfaces, including stainless-steel and plated
material without a primer.
Once
fully cured and in service, Loctite 263 prevents fastener loosening and leakage
caused by shock and vibration, and withstands temperatures up to 360ºF. It
offers excellent resistance to a variety of industrial fluids and solvents,
ensuring a leak-free seal of the threaded assembly. Localized heat and hand
tools are required to disassemble fasteners treated with the threadlocker.
The
product is available in 0.5 ml capsules, 10 ml tubes, and 50 ml, 250 ml or 1
liter bottles.