Henkel Loctite Corp. has introduced Loctite Hysol U-09FL, a robust, high performance urethane adhesive for bonding polycarbonate and a variety of other plastics, as well as glass and metal. It exhibits good storage stability and, once mixed, offers a 10-minute worklife. This two-component urethane cures at room temperature in three to 24 hours. Ultra-clear and highly flexible, it provides strong peel strength and is for applications that require a clear, non-yellowing bondline.