Kaucuk: Pourable Liquid Rubber
April 27, 2000
The recently introduced Krason™ “pourable” liquid polybutadiene rubber is highlighted in this company’s new six-page, pocket-sized brochure. The literature focuses on the many potential applications of the material, including a coagent in the production of electrical-cable sheathing, casting systems, polyurethane coatings and binding material to bridge expansion joints, and electrical-insulation material. The product features excellent hydrophobicity and hydrolytic resistance, good electrical-insulation properties and low-temperature flexibility.