Kraton Polymers has developed Kraton A polymers, an extension of its existing polymer technology. The polymers are high-performance elastomers. The versatility of the polymers is due to their molecular structure, which can be precisely controlled and tailored to perform in specific applications. They can also provide formulation flexibility in commonly used thermoplastic processing technology. The polymers can be compounded to produce materials that improve the strength, elasticity, temperature resistance, softness, appearance, grip and convenience of a diverse range of applications including toys, packaging, automotive, sports, construction and molded and extruded goods.