Lamart Corp., a custom web coating and laminating specialist, offers a new 5 mil. transfer tape that bonds readily to even the roughest surfaces. Transfer Tape 1102-60 has demonstrated a minimum 180 degree peel and loop tack value of 55 oz./in. and 32 oz./in., respectively. This highly durable tape, which employs a 60# polycoated liner, also provides shear strength of greater than 100 hours at room temperature and 60 hours at 200 degrees F.