Master Bond Inc. has introduced a new single-component, high-performance epoxy adhesive called EP13. This compound requires no mixing and has an unlimited working life at room temperature. EP13 has excellent bond strength to similar and dissimilar substrates, and it demonstrates superior dimensional stability with a service operating temperature range of -60 to 450 degrees F. EP13 is 100% reactive and does not contain any solvents or diluents. It can be applied to vertical surfaces without sagging or dripping. It cures at temperatures of 300 to 350 degrees F for 60-90 minutes; the higher the temperature, the shorter the cure time.