MASTERBOND: Optecally Clear UV-Curable Adhesive/Coating

January 13, 2005
Master Bond, Inc. has introduced a new one-component, optically clear, non-yellowing UV-curable polymer called UV15-7. This 100% reactive system does not contain any solvents or other volatiles. UV15-7 cures almost instantaneously when exposed to a source of UV light of adequate wavelength and intensity. It demonstrates excellent adhesion to a range of substrates, from glass and iron to polyester films and polycarbonates. UV15-7 offers superior chemical resistance and electrical insulation properties. Upon cure, it has a shore D hardness of 60 and an elongation of 6-8%.

For more information, visit http://www.masterbond.com or e-mail Main@masterbond.com.