Medical-Grade Light-Cure Adhesive

October 1, 2002
HENKEL LOCTITE CORP.

Loctite[R] 3345 is a high-performance, ultraviolet-cure, medical-grade adhesive designed for metal-to-glass bonding. Offering superior sterilization resistance, this product is ideal for a variety of medical-device assembly applications, including needle assemblies, syringes, oxygenators, filters and reusable medical devices where limited repeat steam sterilization is required. The adhesive complies with ISO-10993 biocompatibility requirements. Circle No. 211