Adhesives Magazine

Medical-Grade PSA Tape by Scapa Medical

March 4, 2003
Medical-Grade PSA Tape by Scapa Medical

This company offers Bioflex Rx100P, a single-coated, medical-grade pressure sensitive adhesive (PSA) tape for direct skin application. Breathable, comfortable and lightweight, the product is ideal for TENS, EKG electrode and bandage applications. Rx100P is supplied on a white, polycoated, stay-flat, easy-release liner that allows for easy die cutting. The medical-grade adhesive system used provides good adhesion to skin, yet removes cleanly without causing skin trauma.